ARI Abstracts
ARI Abstracts hosting, Science for all
 ARI Abstracts ISSN 2960-2483 (Continues: eCM conferences open access online periodical, ISSN 2522-235X- until July 2023)

eCM Meeting Abstracts 2013, Collection 5

5th Symposium on Biodegradable Metals
Umang Island, 25th -31st August 2013

Abstracts

All abstracts: click here to download all the abstracts in one file

Page 1: N Hort, CL Mendis, P Maier
Do we need alloying elements for Mg implant materials?

Page 2: AJ Griebel, JE Schaffer
Development of high-strength bioabsorbable Mg alloys suitable for conventional cold-working processes

Page 3: M Wolff, T Ebel, KU Kainer, T Klassen
Porosity and Young´s-modulus control und measurement on Mg alloy parts, produced by PM (Powder Metallurgy) and MIM (Metal Injection Moulding)

Page 4: KS Shin, HC Jung, MZ Bian, ND Nam, NJ Kim
Characterization of biodegradable magnesium single crystals with various crystallographic orientations

Page 5: Q Peng, H Fu, J Zhang, Y Tian, R Liu
Preparation, mechanical and degradation properties of Mg-based microwire for self-assembly stents

Page 6: KJ Laws, JD Cao, M Ferry
Amorphous alloys – processing, properties and applications

Page 7: E Mouzou, P Agung, A Mostavan, C Paternoster, R Tolouei, S Turgeon, D Dubé, F Prima, D Mantovani
Fe-based alloys with TWIP effect for biodegradable stents

Page 8: A Mostavan, C Paternoster, R Tolouei, E Ghali, D Dubé, D Mantovani
Effect of phosphorus on the corrosion behaviour of electroformed iron-based bilayer materials targeted for biodegradable stent application

Page 9: AH Yusop, NM Daud, H Hermawan
Development of PLGA-infiltrated porous iron for temporary medical implants

Page 10: JA Nordin, NM Daud, DH Prajitno, H Nur, H Hermawan
Synthesis of bovine hydroxyapatite-iron composite via dry mechanochemical process for biodegradable bone scaffolds

Page 11: L Mao, M Kwak, Q Xue, Y Lu, J Niu, J Zhang, G Yuan, R Fan
Stent materials-dependent macrophage fusion and secretion of inflammatory cytokine and chemokine

Page 12: K Hanada, X Huang, K Matsuzaki
Microstructure, mechanical properties and corrosion behaviour of Mg-3Al-1Zn alloy stent tubes

Page 13: AG Demir, B Previtali, V Furlan
Surface structuring of AZ31 Mg alloy with a laser beam for biodegradable stent applications

Page 14: MV Manuel
Magnesium and its alloys – an introduction to their metallurgy and deformation behaviour

Page 15: E Mostaed, Q Ge, M Vedani, PA De Oliveira Botelho, C Zanella, F Deflorian
Mechanical properties and corrosion behaviour of ZK60 processed by ECAP for biomedical application

Page 16: N Huang, SJ Zhou, LS Guo, J Wang
Effect of process on the properties of biodegradble Mg-2Zn-0.2Mn alloy

Page 17: K Bracht, N Angrisani, JM Seitz, R Eifler, A Weizbauer, J Reifenrath
Influence of different storage durations on the properties of degradable magnesium based implants

Page 18: GC Yue, SJ Zhu, LG Wang, X Ma, C Ji, SK Guan
Degradation of Mg-Zn-Ca alloy processed by high pressure torsion for bone implant application in simulated body flood

Page 19: D Liu, L Liu, W Zheng, M Chen
Corrosion and wear behavior of Mg-xZn-0.8Zr alloy in simulated body fluid

Page 20: SK Guan, SJ Zhu, LG Wang, GC Yue, J Wang, J Jin
Microstructures and corrosive properties in simulated body fluid of biological Mg-Zn-Y-Nd alloy by friction stir processing

Page 21: L Jauer, W Meiners, R Poprawe
Selective laser melting of biodegradable metals

Page 22: RK Singh Raman
Mechanical integrity of magnesium-based biodegradable alloys under combined action of stress and corrosive body fluid

Page 23: P Maier, CL Mendis, G Tober, J Briesemeister, E Minciel, N Hort
Bending strength and crack propagation in cast Mg10Gd influenced by corrosion

Page 24: D Liu, L Liu, Y Liu, R Song, M Chen
Effects of grain size on the corrosion resistance of Mg-Zn-Ca Alloy

Page 25: J Wang, V Shanov, ZG Xu, Y Jang, V Giri, B Collins, J Sankar, N Huang,Y Yun
Biodegradation behaviour of magnesium alloy under flow-induced shear stress

Page 26: K Vano-Herrera, F Zimmermann, M Stekker, C Vogt
Investigation of coated magnesium alloys by IR, Raman, X-ray and Mass spectrometry

Page 27: S Natasha, RSP Malon, DHB Wicaksono, EP Córcoles, H Hermawan
Electrochemical detection of magnesium ions using magnesium biosensor

Page 28: S Zhang, X Li, H Wu, C Zhao, J Liu, Y Zhang, X Zhang
Effect of stress on the corrosion behaviour of magnesium wire in m-SBF

Page 29: B Li, Y Han
Nanorod-shaped hydroxyapatite formed on pure magnesium by Micro-arc oxidation and hydrothermal treatment

Page 30: ZJ Jia, M Li, Q Liu, XC Xu, Y Cheng, YF Zheng, TF Xi, SC Wei
Inhibitor-loaded chitosan coatings on the microarc oxidized Mg-1Ca alloy

Page 31: X Zhang, G Yuan, Z Wang, Y Xue
In vitro biocorrosion behavior of NZ20K alloy evaluated by different methods

Page 32: CD Yim, SK Woo, YM Kim, BS You
Corrosion behaviour of Mg-aCa-bY extrusions in simulated body fluid

Page 33: J Zhou, H Gong, D Yao
Absorbable Mg-ND composite and Zn alloy for surgical implant application

Page 34: S Hiromoto, K Hanada, K Matsuzaki
Hydroxyapatite and octacalcium phosphate coating of bioabsorbable Mg-Ca alloys by a novel chemical solution deposition method

Page 35: BJC Luthringer, L Wu, M Costantino, A Burmester, AF Schilling, F Feyerabend,
R Willumeit
In vitro strategies to mimic in vivo events after osseous implantation

Page 36: D Tie, RG Guan, T Cui, LL Wu, LL Song, HM Qin
Influence of strontium concentration on in vitro corrosion property and cytocompatiblity of ternary Mg-Zn-Sr alloys

Page 37: YF Zheng, WR Zhou, L Ruan
In vitro studies on Mg-Ge(-Ca, Zn) alloy system newly-developed for potential biomedical applications

Page 38: K Törne, AN Weissenrieder, J Weissenrieder
Corrosion of zinc in PBS, Ringer solution, blood plasma and whole blood

Page 39: L Yang, Z Zhen, C Lai, TF Xi
Cytotoxicity evaluation of Mg-Sn-Mn alloy on mouse fibroblasts using iTRAQ-based quantitative proteomic analysis

Page 40: H Liu
Degradation and cytocompatibility of magnesium alloys for medical applications – an introduction to methods and observations

Page 41: F Feyerabend, A Möhring, R Willumeit
Preincubation increases in vitro cell adhesion to magnesium and its alloys

Page 42: CA Grillo, F Alvarez, WD Müller, M Fernández Lorenzo de Mele
Assessment of cellular effects in the vicinity of Mg, AZ31 and ZEK100 alloys

Page 43: T Patel, ME Iskandar, H Liu
Bioresorbable metallic interference screws for anterior cruciate ligament reconstruction – an evaluation of mechanical and degradation properties

Page 44: J Zhang, N Kong, HY Li, GY Yuan
Effect of proteins and cells on degradation behaviour of Mg-Nd-Zn-Zr alloy

Page 45: X Lin, LL Tan, C Liu, X Wang, K Yang
Characterization of hydroxyapatite containing micro-arc oxidation coating on ZK60 magnesium alloy

Page 46: MS Dambatta, NS Murni, I Sudin, H Hermawan
The degradation rate and cytocompatibility of Zn-3Mg alloy

Page 47: X Lin, XM Yang, LL Tan, Y Zhang, K Yang
In vitro degradation and biocompatibility of ZK60 magnesium alloy with Sr-containing micro-arc oxidation coating

Page 48: P Tian, XY Liu
Anticorrosion and cytocompatibility of biodegradable polylactide/MgO composite coating on AZ31 alloy

Page 49: NM Daud, H Hermawan
The interaction of fibroblast cells on the surface of porous iron

Page 50: K Bobe, E Willbold, I Morgenthal, O Andersen, J Nellesen, W Tillmann, C Vogt, K Vano, F Witte
Open porous Mg scaffolds show biocompatibility differences at long term

Page 51: J Reifenrath, C Roessig, L Wolters, JM Seitz, P Helmecke, N Angrisani
Implant location strongly influences degradation and applicability of magnesium alloys for orthopaedic application

Page 52: J Zhang, YZ Bi, MF Chen, Y Huang
The degradation behavior of Mg-3Zn-0.5Zr alloy in an in vitro and in vivo environment

Page 53: F Witte, K Bobe, M Meier
MRI based perfusion measurements in bone after implantation of biodegradable magnesium rods

Page 54: A Purnama, M-C Drolet, Jacques Couet, Diego Mantovani
In vivo study of iron-based biodegradable metals using rat model

Page 55: D Paramitha, S Estuningsih, D Noviana, MF Ulum, H Hermawan
Distribution of Fe-based degradable materials in mice skeletal muscle

Page 56: D Noviana, AK Nasution, MF Ulum, H Hermawan
Degradation of Fe-bioceramic composites at two different implantation sites in sheep animal model observed by X-ray radiography

Page 57: D Noviana, AK Nasution, MF Ulum, H Hermawan
Monitoring of early biodegradation of Fe-bioceramic composites by B-mode ultrasonography imaging in sheep animal model

Page 58: DY Zhang, RL Gao, WJ Lin, L Qin, G Zhang, P Cao, H Qiu, GQ Wang, Y Xia
In vitro and in vivo charaterization of a nitrided iron coronary stent

Page 59: MF Ulum, D Paramitha, S Estuningsih, D Noviana, H Hermawan
Metal ion level and polymorphonuclear leukocyte cells number as determination factors for early in vivo rejection of biodegradable metals

Page 60: GJ Dias, J Walker
In vivo Models for the Evaluation of Degradable Metallic Biomaterials for Orthopaedic Applications

Page 61: L Qin
The role of magnesium and associated alloying elements in human physiology and biology

Page 62: BD Xue, ZH Lu, GY Yuan, ZW Xu
Experimental study on stent implantation for congenital tracheal stenosis in infants and children

All abstracts: click here to download all the abstracts in one file